4140 Liga tal-Azzar Falsifikati Bar
Dijametru: 6.500 pulzier
Tolleranza tal-Qtugħ: 0 . 125 pulzier / -0 pulzieri.
Firxa tad-daqs tal-qtugħ: 0 . 375 pulzier sa 72 pulzier f'żidiet ta '0.125 pulzier.
Għal daqsijiet u tolleranzi barra din il-firxa, jekk jogħġbok ikkuntattjana .
Propjetajiet mekkaniċi tipiċi
Brinell Hardness - 269 / 341bhn
Qawwa tat-Tensili - 156, 000 psi
Qawwa tar-Rendiment - 123,500 PSI
Bħala fornitur u manifattur ewlieni fiċ-Ċina, GNEE Steel jipprovdi prodotti ta' liga bbażati fuq in-nikil-kost effettivi.
- Ibgħat E-posta:ss@gneesteel.com
- Tel:+8615824687445
GNEE 4140 Steel Forged Bar Daħħal
4140 Liga tal-Azzar Falsifikati Bar


GNEE Steel tqassam Premium AISI 4140 Alloy Steel Forged Bars u Forgings . L-istokk tagħna huwa disponibbli għal serrar immedjat, qtugħ u konsenja taħt API Q1 u ISO 9001: 2015 Rekwiżiti tas-Sistema ta 'Ġestjoni tal-Kwalità ċċertifikati .
Aħna nilħqu r-rekwiżiti stretti tal-klijenti tagħna b'ħinijiet qosra ta 'ċomb u tibdil mgħaġġel .
4140 Karatteristiċi tal-Bar Falsifikati
AISI / SAE 4140 Alloy Steel huwa azzar ta 'liga baxxa fil-familja tal-kromju-molybdenum . AISI 4140 għandu saħħa għolja, ebusija, ebusija tajba, distorsjoni ta' tkessiħ baxx, saħħa ta 'tkessiħ baxxa, saħħa ta' creep għolja u saħħa ta 'ksur tat-temperatura għolja . AISI 4140 ASSA 4140 AISI għandu kontenut ta' karbon Trattament tas-sħana .
4140 Legs Azzar Falsifikati Il-vireg għandhom firxa wiesgħa ta 'użi fl-aerospazjali, iż-żejt u l-gass, u l-industriji tal-karozzi, u ħafna drabi jintużaw fl-għodod tan-downhole .
GNEE 4140 liga ffalsifikata speċifikazzjoni tal-bar
AISI 4140 Falsifikazzjoni Bar: Propjetajiet Komprensivi
|
Kategorija tal-Propjetà |
Parametru |
Speċifikazzjonijiet |
|---|---|---|
|
Dimensjonijiet |
Dijametru (tond) |
50 - 800 mm |
|
Ħxuna (kwadru / rett) |
50 - 400 mm |
|
|
Wisa '(kwadru / rett) |
50 - 1200 mm |
|
|
Tul |
0.5 - 15 m (±0.1%) |
|
|
Standards |
Ċertifikazzjoni Internazzjonali |
ASTM A668 Klassi F / EN 10250 / DIN 7525 / JIS G4105 |
|
Kundizzjoni tal-wiċċ |
Stat Falsifikat |
Wiċċ miksi bl-iskala (ossidu iswed) |
|
Wara l-ipproċessar |
Makna, mitħuna, jew bl-isparatura |
|
|
Ebusija |
As-Falsifikat (HB) |
197 - 241 |
|
Mkellef & Temprat (HRC) |
28 - 35 |
|
|
Densità |
Proprjetà fiżika |
7.85 g / cm³ |
|
Kompożizzjoni tal-materjal |
Kimika (%) |
C: 0.38-0.43, cr: 0.80-1.10, mo: 0.15-0.25, mn: {0.75-1.00, si: {0.15-0.35, p / s inqas minn jew daqs 0.035 |
|
Applikazzjonijiet ewlenin |
Setturi industrijali |
Xaftijiet tat-Trasmissjoni tal-Qawwa, Hubs tal-Iskrun tal-Baħar, Hammers tal-Minjieri Crusher |
Propjetajiet mekkaniċi u proċessar
|
Proprjetà |
Kif falsifikat |
Q & T ittrattat |
Qligħ tal-prestazzjoni |
|---|---|---|---|
|
Qawwa tat-tensjoni (MPA) |
650 - 800 |
950 - 1200 |
↑46% |
|
Qawwa tar-Rendiment (MPA) |
Akbar minn jew daqs 400 |
Akbar minn jew daqs 720 |
↑80% |
|
IMPATT TA 'L-IMPATT (J) |
50 - 65 |
35 - 45 |
↓30% |
|
Limitu tal-Għeja (MPA) |
240 |
380 |
↑58% |
|
Forġa tal-firxa tat-temp |
1150-850 grad (martell / die) |
- |
Irfinar tal-qamħ ottimali |
Kompożizzjoni kimika standard "4140 grad"
| Karbonju | 0.38-0.43 |
| Manganiż | 0.75-1.00 |
| Fosfru (Max) | 0.035 |
| Kubrit (Max) | 0.040 |
| Silikon | 0.15-0.35 |
| Kromju | 0.80-1.10 |
| Molibdenu | 0.15-0.25 |
Firxiet ta 'proprjetà mekkanika stmati għal "Grad 4140"
| Qawwa tat-Tensili (PSI) | 95,000 - 105,000 |
| Qawwa tar-Rendiment (PSI) | 65,000 - 75,000 |
| Titwil f'2 "(%) | 20 - 30 |
| Tnaqqis taż-żona (%) | 35 - 45 |
| Brinell Hardness (BHN) | 200 - 230 |
Gnee Metal 4140 Alloy Steel Bar Skeda
Rawnds (pulzieri)
| 1/2 | 1-7/8 | 3-1/2 | 6-1/4 | 9 | 14 |
| 5/8 | 2 | 3-3/4 | 6-1/2 | 9-1/2 | 16 |
| 3/4 | 2-1/8 | 4 | 6-3/4 | 9-3/4 | |
| 7/8 | 2-1/4 | 4-1/4 | 7 | 10 | |
| 1 | 2-3/8 | 4-1/2 | 7-1/4 | 10-1/2 | |
| 1-1/8 | 2-1/2 | 4-3/4 | 7-1/2 | 11 | |
| 1-1/4 | 2-5/8 | 5 | 7-3/4 | 11-1/4 | |
| 1-3/8 | 2-3/4 | 5-1/4 | 8 | 11-1/2 | |
| 1-1/2 | 2-7/8 | 5-1/2 | 8-1/4 | 12 | |
| 1-5/8 | 3 | 5-3/4 | 8-1/2 | 13 | |
| 1-3/4 | 3-1/4 | 6 | 8-3/4 | 13-1/2 |
Kwadri (pulzieri)
| 1/2 | 1 | 1-3/4 | 3-1/2 | 6 |
| 5/8 | 1-1/8 | 2 | 4 | |
| 3/4 | 1-1/4 | 2-1/2 | 4-1/2 | |
| 7/8 | 1-1/2 | 3 | 5 |
Flats (pulzieri)
| 1/4 x 1 | 3/8 x 4 | 5/8 x 3 | 1 x 2-1/2 | 1-1/2 x 2-1/2 | 2-1/2 x 3-1/2 |
| 1/4 x 1-1/2 | 1/2 x 1 | 3/4 x 1-1/2 | 1 x 3 | 1-1/2 x 3 | 2-1/2 x 4 |
| 1/4 x 2 | 1/2 x 1-1/2 | 3/4 x 2 | 1 x 4 | 1-1/2 x 4 | 2-1/2 x 6 |
| 1/4 x 3 | 1/2 x 2 | 3/4 x 2-1/2 | 1 x 5 | 1-1/2 x 5 | 3 x 4 |
| 1/4 x 4 | 1/2 x 2-1/2 | 3/4 x 3 | 1 x 6 | 1-1/2 x 6 | 3 x 5 |
| 1/4 x 5 | 1/2 x 3 | 3/4 x 4 | 1-1/4 x 2 | 2 x 2-1/2 | 3 x 6 |
| 1/4 x 6 | 1/2 x 3-1/2 | 3/4 x 5 | 1-1/4 x 2-1/2 | 2 x 3 | |
| 3/8 x 1-1/2 | 1/2 x 4 | 3/4 x 6 | 1-1/4 x 3 | 2 x 3-1/2 | |
| 3/8 x 2 | 1/2 x 5 | 1 x 1-1/4 | 1-1/4 x 3-1/2 | 2 x 4 | |
| 3/8 x 2-1/2 | 1/2 x 6 | 1 x 1-1/2 | 1-1/4 x 4 | 2 x 5 | |
| 3/8 x 3 | 5/8 x 2 | 1 x 2 | 1-1/2 x 2 | 2 x 6 |
Aħna naħżnu AISI 4140 u AISI 4130 Steel in Round, Square and Flat Bar . Il-materjal kollu huwa rrumblat bis-sħana b'finitura tal-wiċċ . jekk jogħġbok ċempel jew ibgħatilna email għal kwotazzjoni b'xejn . Il-materjal imkessaħ u ttemprat, it-temperat, it-temperat, l-istress meħlus u l-istress imtaffi Tulijiet bl-addoċċ tas-saqajn, tulijiet bl-addoċċ 20/24 tas-sieq u għażliet ta 'qtugħ tad-dwana) . 4140 u 4150 ligi huma użati ħafna f'applikazzjonijiet mekkaniċi ta' skop ġenerali . tipikament, 4150 u 4140 bars tondi fuq 10 pulzieri fid-dijametru huma fornuti f'disovità mdawra mhux maħduma .
Ambjent tal-Fabbrika tal-Grupp GNEE
GRNEE GRUP

GRNEE GRUPP 4140 Steel Bar Packaging
GNEE GRUP

Ittestjar tal-Grupp Gnee
Ittestjar tal-BAR GROUP 4140

FAQ
Il-korrużjoni tal-azzar tal-liga 4140 hija reżistenti?
Għalkemm l-azzar 4140 fih kromju biex ittejjeb ir-reżistenza għall-korrużjoni, mhuwiex reżistenti ħafna għall-korrużjoni . kisi xieraq jew miżuri protettivi huma rrakkomandati għall-użu f'ambjenti korrużivi .
X'inhi d-differenza bejn l-azzar tal-liga 4140 u 4340?
4140 L-azzar għandu kontenut ta 'karbonju aktar baxx minn 4340 azzar, li jagħmilha aktar faċli għall-magna . Madankollu, l-azzar 4340 għandu saħħa u ebusija ogħla, speċjalment f'sezzjonijiet ikbar, u ħafna drabi jintuża f'applikazzjonijiet heavy-duty .
L-azzar tal-liga 4140 jista 'jkun iwweldjat?
Iva, l-azzar 4140 jista 'jiġi wweldjat bl-użu tat-tekniki u l-prekawzjonijiet tal-iwweldjar xierqa . Madankollu, it-trattament tas-sħana ta' wara l-weldjatura jista 'jkun meħtieġ biex terġa' tinkiseb il-proprjetajiet tagħha, speċjalment fiż-żona affettwata mis-sħana .
It-tags Popolari: 4140 Liga tal-Azzar Falsifikati Bar, iċ-Ċina 4140 Liga tal-Azzar Falsifikati Fornituri
Par ta ' l-
Bar tal-azzar strutturali tal-liga 15CRMOTista 'Tħobb ukoll
Ibgħat l-inkjesta